Drilling Holes in 3D Printed Parts for Accurate Fits

Drilling holes in 3D printed parts gets a fit the print can't hold. Why printed holes miss size, how to model a pilot, and when to ask for post-machining.

Printed holes are close, not exact. For a bolt clearance hole that's fine. For a pin, a bearing or a press fit, drilling holes in 3D printed parts after printing is how you get the size you actually want.

How Do You Get Accurate Holes in a 3D Printed Part?

Print the hole a little undersize or as a pilot, then drill or ream it to size. Keep the tool and the plastic cool so the material cuts instead of smearing.

The Engineering Way's How to Make Perfect Accurate Holes and Threads in 3D Printed Parts explains the failure: drilling and tapping "generate heat and soften the material, so it moves and smears instead of cutting cleanly." The fix in the description is blowing compressed air into the hole while you cut. That video is about filament printing, but heat and smearing are the same problem in powder-bed nylon.

Why Printed Holes Come Out Off-Size

Our 3D printing tolerance is "±0.3 mm or ±0.3%, whichever is greater." On a small hole that's a lot of room compared to a slip fit. The as-printed surface is also rough enough to change how a pin seats.

HP's machining recommendations for Multi Jet Fusion say a machining post-process can reach tolerances "up to ±0.05 mm" in a particular area. They suggest that when you drill straight to final size you skip the pre-hole and let the machine make it, so the drill lands in the right spot. For larger holes cut by interpolation, they model a pre-hole at least 1 mm under the final diameter.

Drilling Holes in 3D Printed Parts: Practical Rules

  • Model clearance holes to size and don't bother drilling them.
  • For fits, model a pilot and note the finished size on a drawing.
  • Leave enough wall around the hole for the drill to cut into. A thin boss can split. See MJF wall thickness tolerance on thin features.
  • Use sharp drills and light pecks. Dull tools heat the nylon fast.

Stiffer material machines better. HP's note says "Softer and flexible plastics are not suitable for machining," so TPU is out. MJF Nylon, SLS Nylon PA12 and MJF Glass-Filled Nylon are on our Materials page.

Press fits in printed nylon also loosen over time, as covered in why an MJF press-fit boss loosens. If a printed hole needs a finished size, note it on the RFQ and ask us when you quote. For threads, heat-set inserts usually beat drilled-and-tapped nylon.