What Is Shore Hardness?
Shore hardness is a material's resistance to permanent indentation, read from a spring-loaded durometer pressed into the surface. The number only means something next to its scale letter, so a 95A part and a 95D part are very different materials.
In What is Shore Hardness?, Craig from INTERTRONICS walks through the scales. Shore 00 covers very soft materials, like a gel shoe insole. Shore A covers flexible materials such as silicones and harder rubbers, with car tires as his example. Shore D is for less flexible plastics, and he puts human bone at roughly D90. The scales are named after Albert Ferdinand Shore, who invented the durometer.
Where the Scales Overlap
Smooth-On's durometer Shore hardness scale shows how the scales overlap. Its example is that a 95A material is also about 45D. The printed TPUs in our earlier posts sit in the 90s on the A scale, a 92A in one and a 95A in the other, near the top of A where it starts to overlap D. Smooth-On also describes the gauge: a needle on a spring that you press firmly until it has gone as deep as it will go.
The number leaves a lot out. It's a surface indentation test, so it says nothing direct about tear strength or how a part rebounds after a long squeeze. A printed part's feel also depends on geometry as much as material. A study we covered in printed TPU lattices measured a 95 Shore A lattice far softer than the solid TPU it came from.
Putting It on a Drawing
Our post on Rockwell hardness on a drawing explains why a hardness callout works better as a range than a single number, and the same thinking helps when you write a durometer on a print. If your part is a seal, check where printed TPU gaskets work before you settle on a number.