← All posts

Laser Cut Kerf: Should Your DXF Allow for It?

Laser cut kerf is the width the beam removes. Why you should draw a sheet metal DXF at finished size instead of offsetting it, and where kerf affects fits.

Anyone who's run their own laser learns about kerf the first time a finger-jointed box comes out loose. So when it's time to send a steel part to a fabricator, the natural instinct is to shrink the slots in the DXF first. For laser cut kerf on a sheet metal order, that's usually the wrong move.

Should You Compensate for Laser Kerf in Your DXF?

No, not when a shop is cutting it. Draw the part at the finished size you want and let the cutting software offset the beam path. If you shrink the geometry as well, the kerf comes off twice.

LightBurn's Calculating and Applying Kerf Offset shows why kerf matters in the first place. The beam is centered on your line, so half of it cuts inside and half outside. Their example: tell the laser to cut a 25 mm square with a 0.5 mm beam and you get a 24.5 mm square, plus a 25.5 mm hole in the stock. The fix in LightBurn is a kerf offset in the cut settings, which leaves the shape itself alone, and you measure it again for each material because every material cuts differently.

That's software for running your own machine, but the geometry is the same on an industrial laser cutting Cold Rolled Steel or Aluminum 5052. What changes is who sets the offset.

Why Laser Cut Kerf Is the Shop's Job

Kerf width depends on the material and the cut settings, and you can't see any of that from your desk. The shop can. SendCutSend's laser cutting guidelines put it in one line: "Build your file at the exact size you want it cut." The same page lists the minimum internal corner radius for laser cutting as "approximately the kerf width." So even a part drawn at size shows its kerf in one spot: sharp inside corners get a tiny radius.

Where Kerf Still Touches Your Design

Fits. If two of your parts slot together, put the clearance in the drawing as a real gap instead of hoping the beam width supplies it. Tab and slot clearance for laser-cut sheet metal covers how much. Small holes are the other spot, since the kerf is a bigger share of a small feature; see the smallest hole you can laser cut. And if you're not sure which file to send at all, read DXF or STEP for a sheet metal part.

On our sheet metal side, cut tolerance is ±0.13 mm. Send the DXF at 1:1 and finished size, and if a fit depends on how kerf is handled in your material, ask us when you quote.

Need a part made?

Upload your file for an instant price.

Start a quote