Ra vs Rz: Which Roughness Number Goes on the Drawing
Ra vs Rz: Ra averages surface height, Rz averages peak-to-valley, and no chart converts one to the other. Which to call out on a seal face or a fit.
A drawing shows up with Rz 6.3 on a seal face, the shop's profilometer habit is Ra, and somebody goes looking for a conversion chart. That's how most Ra vs Rz trouble starts, because there isn't a conversion that holds up.
What Is the Difference Between Ra and Rz in Surface Roughness Measurement?
Ra is the average distance the surface strays from its mean line. Rz is the average peak-to-valley height, so Ra describes how rough the surface is overall and Rz describes how tall its worst features are.
BRKNDT, a roughness-tester maker, opens the description of Ra vs Rz Explained with exactly that question. The short video makes two points worth keeping. The two numbers can't be directly converted, and you should use whichever parameter the drawing, standard or inspection requirement specifies.
Ra vs Rz on a Real Part
Ra's weakness is that it averages. Keyence's write-up on roughness height parameters shows two surfaces with the same Ra and very different textures, one dominated by sharp peaks and one by deep valleys. A single Ra number can't tell them apart. Rz is built from the extremes, so it reacts far more to a single scratch or torn spot.
That gives you a working rule. Ra is fine for general finish control, and Keyence calls it the most commonly specified parameter on drawings. Reach for Rz where one peak or valley breaks function. Keyence lists sealing surfaces, wear interfaces and parts where a peak could start a failure.
An O-ring face is the classic case. A surface can pass an Ra callout comfortably and still carry one deep drag mark across the seal line. Ra averages that mark away; Rz is far more likely to flag it.
Why the Chart Fails
Keyence notes that the exact definition of Rz depends on the standard you're working under, and names ISO 21920 and ASME B46.1 among the documents that govern how roughness is measured and reported. An older print may carry an Rz from a different definition than the one your instrument uses. If the drawing just says "Rz" with no standard, ask which one before anybody measures.
BRKNDT's other point applies too. Measurement conditions change both readings, so if you're comparing two parts or two suppliers, measure the same surface the same way.
For what a mill leaves before any finishing, see surface finish straight off a 3-axis mill. If finish wanders part to part, why surface finish varies with the same tool covers the usual suspects, and face mill vs end mill matters when the face in question is flat.
Our CNC dimensions default to ISO 2768-m. If you need a measured Ra or Rz reported on a specific face, ask us when you quote.
Need a part made?
Upload your file for an instant price.