← All posts

Threaded Inserts in Machined Plastic: When to Use

Threaded inserts in machined plastic make sense when a screw comes out often or carries real torque. Which insert type fits Delrin, Nylon 6 or PTFE parts.

A tapped hole in plastic works fine the first time. By the tenth time the screw comes out, it's often loose. Threaded inserts in machined plastic fix that, but they aren't free, so it's worth knowing when they earn their place.

When Should a Machined Plastic Part Get a Threaded Insert?

Use one when the joint gets taken apart more than a few times, when the screw needs real clamping torque, or when the plastic is too soft to hold a thread. For a screw that goes in once and stays, a well-sized tapped hole is usually enough.

Pipeline Design & Engineering's Mechanical Design: Threaded Inserts Discussion frames the question this way: plastic parts "can be directly threaded, but they are weak," so a metal insert gives "the lower cost and weight associated with a plastic part, but the higher strength of steel threads."

Which Threaded Inserts in Machined Plastic Fit Which Job?

Machined parts can't use molded-in inserts, so the choice is between installed types.

Heat-set. A heated tool melts a thin layer around the knurls and the plastic flows back in. Delrin CNC's rules for threads and tapped holes in Delrin calls heat-set "the usual choice on machined acetal" and says to "Get the receiving hole diameter from the insert manufacturer rather than guessing."

Press-fit. Cheap and quick, but the same article warns they "rely entirely on interference, which acetal will relax over time through creep." Fine for low loads, not for a joint that matters.

Helical coil. Tapped oversize, then a wire coil wound in. Good where threads see wear, and it's the usual repair for a stripped hole.

Material Matters

On our Materials page, the CNC plastics are Delrin, Nylon 6 and PTFE. Delrin machines cleanly and holds an insert hole well. Nylon 6 takes on moisture, and a hole sized dry can change. PTFE is soft and creeps, so tapped threads in it are weak and inserts need care. See why tight tolerances fail in PTFE and Delrin vs Nylon 6.

Getting It Quoted

Model the insert's receiving hole to the manufacturer's spec and name the insert part number on the drawing. We machine Delrin, Nylon 6 and PTFE on our CNC side. Note the insert type and part number on the RFQ, and ask us when you quote about how the inserts get installed. For printed nylon, the hole rules are different, as in heat-set insert hole size for SLS and MJF.

Need a part made?

Upload your file for an instant price.

Start a quote