Chem Film vs Anodize for Machined Aluminum Parts

Chem film vs anodize on machined aluminum: chem film stays conductive and adds almost no thickness, anodize insulates and wears better. How to choose.

The chem film vs anodize choice usually gets made by habit. Whoever drew the last housing picked one, and the next drawing copies the note. That holds up right until a ground strap won't make contact or a wear face scuffs through in a month.

Should You Pick Chemical Conversion Coating or Anodizing for Your Aluminum Parts?

Start with conductivity. Chem film leaves aluminum electrically conductive, and anodize turns the surface into an insulator, so a part that has to ground or bond through a joint wants chem film there, while a part that needs wear resistance or color wants anodize.

That's how Brett frames it in Protocase's Chemical Conversion Coating vs Anodizing, aimed at viewers trying to decide which of the two suits their parts. He calls conductivity the primary difference. He also points out that chem film is for aluminum only, while anodizing works on titanium and magnesium too.

Chem Film vs Anodize on a Toleranced Feature

Valence Surface Technologies' comparison puts numbers on the thickness side. A chromate conversion layer runs about 250 to 1,000 nanometers, which is next to nothing on a machined fit. Type II sulfuric anodize runs about 0.0001 to 0.001 in., and Type III hard anodize 0.0005 to 0.004 in., growing both into and out of the base metal. On a bore held to a few tenths, that's the difference between ignoring the finish and machining around it.

Valence also notes chem film is soft and can be damaged by handling or abrasion. Don't put it on a surface that rubs and expect it to last.

Where Drawings Go Wrong

Cosmetics come first. Brett says chem film won't hide machining marks. Scratches and swirl marks show straight through, so Protocase recommends a grained or vibratory finish before it goes on.

Then the callout. MIL-DTL-5541 chem film takes a Type and a Class. Type II is the chemistry without hexavalent chromium (not to be confused with Type II anodize), and Class 3 is the one meant for low electrical resistance. A note that just says "chem film" leaves the finisher guessing.

Using both is normal. Valence says many assemblies are anodized overall with the bonding areas masked and chem filmed instead. Draw those pads clearly and nobody has to guess.

If you're going the anodize route, read Type II vs Type III anodize and how much stock to leave for anodizing. The stainless version of this conversation is stainless steel passivation.

Aluminum 6061 and Aluminum 7075 are both on our CNC materials list. Finishing isn't listed on that page, so for chem film or anodize, or both on one part, ask us when you quote.