DMLS Inconel 718: When a Printed Superalloy Pays
DMLS Inconel 718 pays off when the shape can't be machined, but the heat treatment and finish machining after the build decide whether the part is done.
Inconel 718 is miserable to machine and great at living hot. DMLS Inconel 718 looks like the obvious way out: print the shape and skip hours of slow cutting. It can work, but only when the part needs what printing gives, and only if you plan for what happens after the build.
Can Inconel 718 Be 3D Printed?
Yes. Laser powder bed fusion prints it routinely, but it isn't a forgiving alloy, and a part straight off the plate usually isn't finished. Expect heat treatment, often including HIP on critical parts, plus machining on any surface that has to fit something.
Modo Rapid, a metal printing supplier, asks the question in Can Inconel 718 be 3D printed and answers that it can, but it's not for beginners. Its list of problems is specific. Steep temperature gradients leave residual stress that can warp or crack the part, and poor powder or the wrong laser power leaves porosity. Surfaces often need CNC finishing or polishing. By the video's account, heat treatment and hot isostatic pressing (HIP) are usually required to reach aerospace-grade properties.
What the Research Says About DMLS Inconel 718
A NASA study built sixteen commercial 718 powder lots with the same build and heat-treat parameters. Every lot met the 718 chemistry spec, and the parts still showed a wide range of build quality and microstructure. Carbon content in the powder tracked closely with final grain size and strength. The same paper notes that L-PBF tuned for 718 can generally keep porosity under 0.5%, and that parts for critical service may get HIP to close what's left and even out the grain structure.
So "Inconel 718" on a quote isn't the whole spec. For a part that matters, powder certification and the heat-treat route belong on the drawing or the PO, which matches the video's own buyer advice.
When Printing It Pays
Printing earns its keep when the geometry can't be cut, such as internal cooling channels or thin-walled manifolds that would be mostly chips from bar. When DMLS beats CNC walks through that call. Unlike support-free SLS and MJF nylon, a metal powder-bed part is anchored to its plate with supports, and those have to come off. Leave stock on faces that get machined after heat treat; heat treat before or after CNC explains why.
DMLS Inconel 718 is on our 3D printing material list, quoted at ±0.3 mm or ±0.3%, whichever is greater, and the page shows printed metal parts barrel tumbled to break edges. Stress relief, HIP, powder certs, CT inspection and finish machining aren't listed on that page, so ask us when you quote.
Need a part made?
Upload your file for an instant price.