Is Stainless Steel Magnetic? Why 304 Sometimes Is
Annealed 304 and 316 barely pull a magnet, but bends and cut edges can. Why some stainless steel is magnetic and how to spec a part that must not be.
K&J Magnetics sells magnets, so it's fair that they asked the question in a video title: is stainless steel magnetic? They answered it the direct way, by sticking a neodymium magnet to several grades and measuring the pull.
Is Stainless Steel Magnetic?
Some of it is. Austenitic grades like 304 and 316 are close to non-magnetic when annealed, while other families pull a magnet well, including precipitation-hardening grades like 17-4 PH.
In Is Stainless Steel Magnetic?, a piece of 304 bar stock had a little pull, and it seemed to be only at the edges. The ferritic 430 was plainly magnetic. They then measured pull force. A 5/8 in by 1/8 in disc pulled about 7.7 lb on the thicker regular steel sheet and about 7.4 lb on the thicker 430. With a bigger 1 in by 1/2 in disc the gap opened up, around 24 lb against about 19.5 lb. Their explanation is that the stainless saturates at a lower field strength than plain steel.
Why 304 Turns Magnetic at Edges and Bends
The British Stainless Steel Association's note Is stainless steel non-magnetic? explains the edge effect. A fully austenitic steel has a relative permeability of 1, but real austenitic grades usually carry a little ferrite or martensite and often land around 1.05 to 1.1. Cold work raises the martensite. Their example is a stainless sink, where the flat drainer barely reacts and the pressed bowl reacts more, most of all in the corners.
So a magnet sticking to a 304 edge doesn't mean the bar is fake. On a machined part, heavily worked areas can pick up some response, which ties into drilling 304 without work hardening it. On bent sheet, the bend lines are where you'd expect it.
Choosing a Grade When Magnetism Matters
If a part sits near a sensor or has to stay "non-magnetic," a grade name isn't enough. The BSSA notes that for jobs like MRI, the customer and supplier agree a maximum permeability, sometimes as low as 1.004. Put that number on the drawing. For the 304 vs 316 choice on corrosion and cost, see 316 vs 304 stainless, and for rust on fresh parts, stainless steel passivation.
What We'd Do on Your Part
Stainless 304 and Stainless 316 are on our Materials list for CNC and sheet metal, with DMLS Stainless 316L and DMLS Stainless 17-4 PH for printing. Expect the 17-4 PH to be magnetic. Permeability testing isn't listed on the site, so if your part carries a limit, ask us when you quote.