Masking Threaded Holes Before Powder Coating Sheet Parts
Masking threaded holes before powder coating: blind holes take tapered plugs, through holes take pull plugs. What your sheet metal drawing should say.
Powder goes everywhere the charge can reach, and that includes the threads you were planning to put a screw into. Masking threaded holes is the coater's job on the day, but whether it gets done right usually depends on what the drawing told them.
How Do You Mask Threaded Holes Before Powder Coating?
With silicone plugs sized to the inside diameter of the thread. A blind hole gets a tapered push plug, and a through hole gets a pull plug that seals both ends. Tape can do it, but plugs are faster and more consistent.
That's the short version of Echo Engineering's How To Mask Threaded Holes before Powder Coating. The presenter measures the thread's inside diameter with calipers, picks a tapered plug whose middle diameter matches it, then pushes and twists it in. For a through hole, the pull plug runs slightly bigger than the thread ID and gets pulled through. He sticks with silicone because it handles the cure temperature better than most other rubbers.
Masking Threaded Holes on a Sheet Metal Drawing
The coater picks the plug. The designer decides what needs one.
Say which holes stay bare. Fabcon's guide to assembly-ready powder coating says masking decisions belong on the drawing at design review, not left to the coater. If the print is silent, somebody is guessing.
Say whether the chamfer matters. Echo's video shows a standard pull plug leaves the leading chamfer coated. A flanged plug is needed when a customer or quality standard wants it bare too.
Settle the hardware order. Fabcon notes that PEM hardware pressed into a pre-coated hole without masking around it loses clinching engagement. It also says standard powders cure at 350 to 400°F part temperature, which rules out some seals, adhesives and pressed-in inserts going in first. Decide whether the PEM nut or the powder comes first before the blank is cut.
Don't count on chasing threads afterward. Running a tap through a coated hole can chip the finish around the opening and expose bare steel, per Fabcon. On Cold Rolled Steel, that's where the rust starts.
Keep the list short. The same guide says a part with 12 masked features can cost more to mask than to coat. If a hole doesn't really need to stay bare, leave it off.
For sheet too thin to tap, see rivet nut vs PEM nut. If you're still choosing the base metal, cold rolled or galvanized steel and galvanized cut edges cover corrosion before any powder goes on.
Our sheet metal work covers laser cutting, press-brake forming and PEM insertion, with ±0.13 mm on cut features. Powder coating isn't listed on that page, so if you need parts coated and masked, ask us when you quote.
Need a part made?