Mill Test Report: How to Read the Cert on Your Metal
A mill test report ties your metal to one heat and lists its tested chemistry and mechanical values. Here's what each block on the cert means for a part.
Ask for certs on a machined part and you'll get a mill test report, often three pages of fine print in more than one language. Most of it is there for a reason, and once you know where to look you can check it against your drawing in a couple of minutes.
How Do You Read a Mill Test Report?
Start with the heat number, then compare the actual test values against the required values printed beside them. A mill test report (MTR) certifies that one heat of metal, made to a named spec, met that spec's chemistry and mechanical requirements, and it shows the numbers to prove it.
Michael of Michlin Metals walks through a real one in How do you Read a Mill Test Report, a three-page cert from an Italian mill for 321/321H stainless. The layout he describes is typical.
The Blocks on a Mill Test Report
The header carries the customer and order details, which you can mostly skip. Below it is the long list of specifications the material is certified to, with revision levels, the UNS designation and the condition. Then comes the identity of the material: shape, size, length, heat number, piece count, weight and lot number. He notes the lot is the portion of the heat processed to that size and condition at one time.
Page two holds the test results. Mechanical properties and hardness show the required values with the actuals from the test on that heat lot underneath. Grain size follows.
Chemistry is the part people misread. Requirements sit in fine print above the actual values, and the numbers are weight percent from samples taken from the melt. Elements listed are either required or restricted by the spec, but not always. On his example, cobalt is listed even though the spec neither requires nor restricts it, so don't treat every line as a pass/fail item.
The footer lists the mill's quality system registrations and who signed off.
What Type of Cert Is It?
European certs are usually issued to EN 10204. According to the Wikipedia summary of mill test reports, a 3.1 certificate comes from the manufacturer with test results, while a 3.2 adds an inspector independent of production, from the purchaser or named in the regulations. If your customer flows down a 3.2, say so before the material is bought, not after.
Specs like 316 vs 304 stainless or 4140 annealed vs prehard are exactly where the cert earns its keep, since the condition line tells you what you actually got. The cert won't tell you about surface condition after machining, which is a passivation question.
What We'd Do on Your Part
We machine from 12 stock materials listed on our Materials page, including Stainless 316 and Alloy Steel 4140. Material certs aren't covered on the site, so if your part needs an MTR with traceability to the heat, ask us when you quote.
Need a part made?
Upload your file for an instant price.