Thermal Expansion: Does Shop Temperature Move Your Part?
Thermal expansion grows a 100 mm steel part about 0.011 mm over a 10 °C swing. When shop temperature matters and why parts are measured at 20 °C.
Jon's Workshop put a blunt question in a video title: does temperature change affect accuracy in a home workshop? He answers it inside the first minute. Yes, because of thermal expansion, and how much it matters comes down to how long the feature is and how far the temperature swings.
Does Temperature Change Affect Machining Accuracy?
Yes. Metal grows as it warms, so a part cut or measured at one temperature reads differently at another. On long features or tight bands it can eat the whole tolerance.
In Does Temperature Change Affect Accuracy in a Home Workshop, Jon, who says he's worked on measurement problems in aerospace and shipbuilding, runs the formula: change in length equals the coefficient times the length times the temperature change. Using 11 millionths per °C for steel, a 100 mm block over a 10 °C day-to-night swing grows about 0.011 mm. A 13 m steel panel from his shipyard work moves about 1.43 mm over the same swing.
He also set three indicators on his mill and came back days later. The weather stayed stubbornly steady and the shop dropped only a couple of degrees. The needles moved roughly 10 to 15 microns, which he fairly calls inconclusive.
How Much Thermal Expansion Matters on a Real Part
Material matters as much as length. The Wikipedia thermal expansion table lists aluminium at 23.1 millionths per °C against 10.8 for carbon steel, so aluminum moves about twice as far. At that rate a 500 mm aluminum plate grows about 0.12 mm over 10 °C. Jon's aluminum example uses a higher coefficient and lands near 0.16 mm. Either way, a plus or minus one or two thou hole spacing is gone.
That's why sizes have a reference temperature. NIST's history of the standard, 20 °C: A Short History of the Standard Reference Temperature, notes that since 1931 industrial lengths have been defined as the size at 20 °C. A part fresh off the machine and still warm will read big until it cools.
What Helps
Jon's advice is practical. Finish the tight features in one setup at one time, and leave non-critical work for another day. Machine a datum feature, such as a dowel hole, so you can pick it up again if the job sits overnight. We'd add one habit of our own: let parts reach room temperature before final inspection.
On the drawing side, see our posts on ISO 2768 general tolerances and tolerance stack-up. If a long aluminum part also moves after roughing, that's stress rather than heat, covered in 6061-T651 plate that still moves.
What We'd Do on Your Part
Our CNC page lists ISO 2768-m as standard, down to ±0.01 mm where the drawing calls for it. That band is 0.02 mm wide, and the steel block above uses about half of it on a 10 °C swing. If you need inspection reported at a stated temperature, ask us when you quote.
Need a part made?