← All posts

HIP for DMLS Parts: When Metal Prints Need It

HIP for DMLS parts closes internal pores and relieves stress, but most metal prints don't need it. When fatigue or a fracture-critical spec makes it pay.

Metal printing specs often carry a line that says "HIP per..." and nobody on the project remembers why. Before you pay for HIP for DMLS parts, it helps to know what the process fixes and what it leaves alone.

Is Hot Isostatic Pressing (HIP) Always Required for Metal Prints?

No. HIP isn't required to get good properties and density from a well-run metal print, but it's worth adding when the alloy or the part's duty calls for it, usually fatigue or fracture-critical service.

That's the answer from a GE Additive (now Colibrium Additive) senior materials engineer in Is Hot Isostatic Pressing (HIP) process always required?, part of the company's Material Myth Conceptions series. He describes HIP as high temperature plus high-pressure inert gas, used to close voids in metal parts. It came from powder metallurgy and castings, where voids are part of the process. His point is that additive parts don't automatically need it, and you should decide based on the alloy and the component requirements.

What HIP for DMLS Parts Actually Changes

Laser powder bed parts can carry small internal pores and residual stress from the build. HIP squeezes the internal pores shut and relieves stress, and in fatigue that's what pays.

NASA's Technical Handbook for AM hardware (NASA-HDBK-5026) lists HIP among the ways to improve AM fatigue life, "to reduce residual stresses and close internal defects," alongside machining the surface and peening. It also flags a catch. For fracture-critical parts, NASA wants a volumetric scan before HIP, because HIP can squeeze a flaw closed without fusing it, and then it's hard to find afterward.

HIP also does nothing for the as-built surface. If a fatigue crack is going to start at a rough downskin face, the fix there is machining, not the furnace.

When We'd Ask About HIP

A printed fixture bracket or a low-stress housing in DMLS Aluminium AlSi10Mg rarely needs it. A cyclically loaded bracket in DMLS Titanium Ti6Al4V, or a hot-section part like the ones in DMLS Inconel 718, is where specs tend to call for HIP and where it earns its cost.

Design still matters more than post-processing. The support structure rules decide where the rough faces end up, and if the part only needs to be strong and simple, machining from bar may skip the question entirely.

What We'd Do on Your Part

Our 3D printing page lists five DMLS alloys, and printed metal parts go through a barrel tumbler to break edges. HIP and stress relief aren't listed there, so if your drawing calls for HIP, ask us when you quote.

Need a part made?

Upload your file for an instant price.